MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
LyondellBasell BMC 695 Vinyl Ester Molding Compound
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Vinyl Ester; Vinyl Ester Sheet Molding Compound

Material Notes: BMC 695 vinyl ester molding compound is a mineral filled glass fiber-reinforced vinyl ester compound suitable for compression and injection molding It is characterized by good moldability, oil and solvent resistance and creep resistance at elevated temperatures.

Typical applications include replacements for die castings and sheet molding compounds, valve covers, timing chain covers, and engine top covers.

LyondellBasell has acquired A. Schulman, Inc..

Vendors:
Available Properties
  • Specific Gravity
  • Specific Gravity
  • Water Absorption, 24 hours, 23°C
  • Linear Mold Shrinkage
  • Linear Mold Shrinkage
  • Hardness, Barcol
  • Tensile Strength
  • Tensile Strength, Ultimate
  • Flexural Strength
  • Flexural Strength
  • Compressive Strength
  • Compressive Strength
  • Izod Impact, Notched
  • Izod Impact, Notched (ISO)
  • Dielectric Strength
  • Dielectric Strength, Short Time
  • Arc Resistance
  • Arc Resistance
  • Comparative Tracking Index
  • Comparative Tracking Index
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Flammability, UL94
  • Flammability, UL94
  • Flammability, UL94
  • Mold Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
LyondellBasell, A. Schulman, former BMC - Bulk Molding Compounds Inc.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.