MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
AISI 1137 Steel, oil quenched from 855°C (1570°F), 540°C (1000°F) temper, round
Categories: Metal; Ferrous Metal; Carbon Steel; AISI 1000 Series Steel; Medium Carbon Steel

Material Notes: Medium strength and good machinability. Applications include spline shafts, and studs, bolts, and nuts with machined threads. Post oil quenched hardness: 48 HRC surface, 43 HRC half-radius, 42 HRC center.

Key Words: UNS G11370, AMS 5024 C, ASTM A29, ASTM A108, ASTM A311, FED QQ-S-637 (C1137), SAE J403, SAE J412, SAE J414
Vendors:
Available Properties
  • Density, Typical for steel.
  • Hardness, Brinell
  • Hardness, Brinell
  • Hardness, Brinell
  • Hardness, Brinell
  • Hardness, Knoop, Converted from Brinell
  • Hardness, Knoop, Converted from Brinell
  • Hardness, Knoop, Converted from Brinell
  • Hardness, Knoop, Converted from Brinell
  • Hardness, Rockwell B, Converted from Brinell
  • Hardness, Rockwell B, Converted from Brinell
  • Hardness, Rockwell B, Converted from Brinell
  • Hardness, Rockwell B, Converted from Brinell
  • Hardness, Rockwell C, Converted from Brinell hardness. Value below normal HRC range, for comparison purposes only.
  • Hardness, Rockwell C, Converted from Brinell hardness. Value below normal HRC range, for comparison purposes only.
  • Hardness, Rockwell C, Converted from Brinell hardness. Value below normal HRC range, for comparison purposes only.
  • Hardness, Rockwell C, Converted from Brinell
  • Hardness, Vickers, Converted from Brinell
  • Hardness, Vickers, Converted from Brinell
  • Hardness, Vickers, Converted from Brinell
  • Hardness, Vickers, Converted from Brinell
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Tensile Strength, Yield
  • Tensile Strength, Yield
  • Tensile Strength, Yield
  • Elongation at Break, in 50 mm
  • Elongation at Break, in 50 mm
  • Elongation at Break, in 50 mm
  • Elongation at Break, in 50 mm
  • Reduction of Area
  • Reduction of Area
  • Reduction of Area
  • Reduction of Area
  • Modulus of Elasticity, Typical for steel
  • Bulk Modulus, Typical for steel.
  • Poissons Ratio, Typical For Steel
  • Shear Modulus, Typical for steel.
  • Izod Impact, annealed at 790°C (1450°F)
  • Izod Impact, normalized at 900°C (1650°F)
  • Izod Impact, as rolled
  • Electrical Resistivity, condition of specimen unknown
  • CTE, linear, Typical steel
  • CTE, linear, Typical for steel
  • CTE, linear, Typical for steel
  • Specific Heat Capacity, Typical steel
  • Thermal Conductivity, Typical steel
  • Carbon, C
  • Iron, Fe, As remainder
  • Manganese, Mn
  • Phosphorus, P
  • Sulfur, S
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.