| Medium viscosity, 10%GF, 1.5mm V0 Uses: E&E/ Security/ Low-voltage apparatus Appearance: Non-transparent Forms: Pellets Processing Method: Injection molding Product ID: BH8095XC Business Unit: Plastics Plastic Manufacturing Process: Medium Viscosity Information provided by Wanhua Chemical Group Co., Ltd. |