MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
LyondellBasell Adflex Z 108S Thermoplastic Polyolefin
Categories: Polymer; Film; Thermoplastic; Polyolefin

Material Notes: Adflex Z 108 S is a reactor TPO (thermoplastic polyolefin) manufactured using the proprietary Catalloy process technology from LyondellBasell. Adflex Z 108 S features a very high softness, a very low flexural modulus and a high melt flow rate. It is used for injection molding, impact modification, extrusion coating, soft compounding, film and fiber applications. It is also selected for the modification of polypropylene homopolymer and random copolymer without altering the transparency. The grade is available in natural pellet form. Commercial: Active Availability Europe; North America; South & Central America. Application: Carpet Backing; Filament Yarn; Hygiene Nonwoven; Impact Modification; Pipe Coating; Roofing Underlayment; TPO Foils and Skins Market Flexible Packaging; Industrial, Building & Construction; Textile Processing Method Cast Film; Compounding; Continuous Filament/Spinning; Extrusion Coating; Injection Molding; Spunbond. Attribute: High Elongation; High Flow; Low Hardness; Low Temperature Impact Resistance; Narrow Molecular Weight Distribution.

Information provided by LyondellBasell.

Vendors:
Available Properties
  • Density, ISO 1183-1
  • Melt Flow, ISO 1133-1
  • Hardness, Shore D, ISO 868
  • Tensile Strength at Break, ISO 527-1,-2
  • Tensile Strength, Yield, ISO 527-1,-2
  • Elongation at Break, ISO 527-1,-2
  • Elongation at Yield, ISO 527-1,-2
  • Flexural Modulus, ISO 178
  • Charpy Impact, Notched, ISO 179, failure mode-complete break
  • Charpy Impact, Notched, ISO 179, failure mode-partial break
  • Charpy Impact, Notched, ISO 179, failure mode-partial break
  • Impact Test, Multi-axial Impact Strength, failure mode-ductile, ASTM D3763
  • Impact Test, Multi-axial Impact Strength, 2.2m/s,3.2 mm plaque, failure mode-ductile, ASTM D3763
  • Tear Strength, ASTM D624
  • Melting Point, ISO 11357-3, DSC
  • Deflection Temperature at 0.46 MPa (66 psi), ISO 75B-1,-2, unannealed
  • Vicat Softening Point, ISO 306, A50
  • Haze, ASTM D1003
  • Gloss, ASTM D2457, @60°
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
LyondellBasell LYB (former Equistar)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.