MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Specialty Compounds RTP Company
LyondellBasell Hostacom™ RTA3184 Thermoplastic Polyolefin Elastomer  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Olefinic Elastomer (TPO); Polyolefin

Material Notes: Description: Hostacom™ RTA3184 medium melt flow, 1,300 MPa flexural modulus, low level glass-reinforced, colorable, interior trim grade thermoplastic elastomeric olefin (TEO) resin is modified to provide balanced rigidity, dimensional stability and processability. It was designed for a variety of molded-in color automotive interior trim components. Uses: Automotive interior parts

Information provided by Basell.

Vendors:
Available Properties
  • Density, ASTM D792
  • Melt Flow, ASTM D1238, Condition L
  • Hardness, Shore D, ISO 868
  • Tensile Strength, Yield, ASTM D 638
  • Tensile Strength, Yield, ISO 527-1, 2
  • Elongation at Break, ASTM D 638
  • Elongation at Yield, ISO 527-1, -2
  • Flexural Modulus, ASTM D790, Tangent, 0.05 in/min
  • Flexural Modulus, ISO 178
  • Izod Impact, Notched (ISO), ISO 180
  • Izod Impact, Notched (ISO), ISO 180
  • Izod Impact, Notched (ISO), ISO 180
  • Gardner Impact, ASTM D3029
  • Gardner Impact, ASTM D3029
  • Tear Strength, ASTM D624
  • CTE, linear, ASTM D696
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648, Unannealed
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648, Unannealed
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75A-1, -2, Unannealed
  • Shrinkage, Basell Test Method, Tool, 100x150x3.2 mm, injection molded plaque
  • Shrinkage, Basell Method, Afterbake, 100x150x3.2 mm
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic
Thermoplastic Elastomer

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Master Bond adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.