MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
NatureWorks® Ingeo™ 3D870 3D Printing Biopolymer
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Renewable/Recycled Polymer; Thermoplastic; Polylactic Acid (PLA) Biopolymer

Material Notes: Ingeo 3D870 is a grade developed for manufacturing 3D printer monofilament. Engineered to deliver improved heat-resistance and high impact strength to 3D printed parts, this formulated grade achieves thermal and mechanical properties similar to ABS while offering an alternative to styrenic-based materials. Monofilaments made with Ingeo 3D870 provide excellent 3D printing characteristics such as precise detail, good adhesion to build plates, less warping or curling, and low odor.

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Melt Flow, ASTM D1238
  • Tensile Strength, ASTM D638, ZX AXIS
  • Tensile Strength, ASTM D638, YX AXIS
  • Tensile Strength, ASTM D638, XY AXIS
  • Tensile Modulus, ASTM D638, YX AXIS
  • Tensile Modulus, ASTM D638, ZX AXIS
  • Tensile Modulus, ASTM D638, XY AXIS
  • Flexural Strength, ASTM D790, ZX AXIS
  • Flexural Strength, ASTM D790, YX AXIS
  • Flexural Strength, ASTM D790, XY AXIS
  • Flexural Modulus, ASTM D790, YX AXIS
  • Flexural Modulus, ASTM D790, ZX AXIS
  • Flexural Modulus, ASTM D790, XY AXIS
  • Izod Impact, Notched, ASTM D256, ZX AXIS, crystalline
  • Izod Impact, Notched, ASTM D256, ZX AXIS, amorphous
  • Izod Impact, Notched, ASTM D256, YX AXIS, amorphous
  • Izod Impact, Notched, ASTM D256, amorphous, XY AXIS
  • Izod Impact, Notched, ASTM D256, YX AXIS, crystalline
  • Izod Impact, Notched, ASTM D256, XY AXIS, crystalline
  • Melting Point, ASTM D3418, Peak
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM E2092
  • Glass Transition Temp, Tg, ASTM D3418
  • Processing Temperature, Compression Section
  • Processing Temperature, Metering Section
  • Feed Temperature, Throat
  • Feed Temperature
  • Adapter Temperature
  • Die Temperature
  • Melt Temperature
  • Drying Temperature
  • Moisture Content
  • Dew Point
  • Drying Air Flow Rate
  • Screw Speed
  • Annealing Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
NatureWorks LLC

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.