| An acrylic self-crosslinking dispersion with complex morphology. The product has low VOC content, it does not contain any APEO emulsifiers or solvents. Dispersion characteristics: - Fast hardening
- Low water absorbability
- Very good anti-blocking
- Very good flexibility
- UV radiation resistance
Application: wood enamels elements of windows and doors, primers and topcoats, wooden facade paints, varnishesInformation provided by Synthos |