MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Specialty Compounds RTP Company
KLJ Group KANATOL 8A Plasticizer
Categories: Fluid

Material Notes: Properties: DOA is almost colourless and odorless oily liquid, free of foreign materials. Does not dissolve in water, dissolves in organic solvents, like the chloroform, gasoline, ethyl acetate, methanol, toluene, mineral oil, vegetable oil, etc; slight soluble in ethylene glycol.

Application: DOA is a highly efficient plasticizers which imparts excellent low temperature flexibility and resistance to impact to the base resin. For these reasons it finds wide use in polymeric systems based on vinyl, nitrocellulose and rubber . It is extensively used in food contact application. In addition to its high efficiency and contribution to the low temperature properties of vinyl DOA is chemically stable and resistant to discoloration on extended exposure to heat and ultraviolet light. The combination of low viscosity and efficiency provide excellent dry blending and processing characteristics. When used in plastisols, DOA imparts low initial viscosity and good viscosity stability.

Chemical Name: Bis ( 2-Ethylhexyl ) Adipate

Molecular Formula: C 22 H42 O4

Molecular Structure: (CH2 ) 4 (COOC 8 H 17) 2

CAS Number: 103-23-1

Information provided by KLJ Group

Vendors:
Available Properties
  • Specific Gravity, ASTM D1045-08
  • Viscosity, KLJ TM-P-13-97
  • Molecular Weight
  • Volume Resistivity
  • Boiling Point, IS 5298-05
  • Pour Point
  • Refractive Index, ASTM D1045-08
  • Moisture Content, ASTM E203-08
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Master Bond adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.