| High heat resistance, High gloss, Excellent impact performance Uses: General Purpose Appearance: Non-transparent Forms: Pellets Processing Method: Injection molding Product ID: N18M2BOU CAS # 25971-63-5; 9003-56-9; Trade Secret Business Unit: Plastics Plastic Manufacturing Process: High Gloss; Good heat resistance; Good impact resistance Information provided by Wanhua Chemical Group Co., Ltd. |