MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Online Metals
Visit Online Metals for fast service
on small quantity orders.
Borealis NAV128-03 PP, post-industrial recycled
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: NAV128-03 is a transparent dark polypropylene (PP) post-industrial recycled supplied in pellets. This product is an ideal PP used where sustainability and circularity matter. NAV128-03 consists of post-industrial waste coming from Borealis plants. Due to the nature of recycled, some variation in color can be observed between batches.

Typical characteristics:

  • Good stiffness / impact balance
  • Low odor
  • Good demolding properties
  • Available in homogenized 12-ton batches
Applications:
  • Injection molding applications

Information provided by Borealis AG

Vendors:
Available Properties
  • Density, ISO 1183
  • Melt Flow, ISO 1133
  • Ash, ISO 1172
  • Tensile Strength, Yield, ISO 527-2, 50 mm/min
  • Tensile Modulus, ISO 527-2, 1 mm/min
  • Charpy Impact, Notched, ISO 179-1/1eA
  • Shrinkage
  • Melt Temperature
  • Mold Temperature
  • Hold Pressure
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.