Temper: Light Drawn, Light Cold Rolled Fabrication Properties: Excellent Suitability – Soldering, Brazing, Gas Shielded Arc Welding, Butt Weld; Good Suitability – Coated Metal Arc Welding, Spot Weld, Seam Weld, Capacity for Being Cold Worked, Capacity for Being Hot Formed; Fair Suitability – Oxyacetylene Welding Common Fabrication Processes: Forming and Bending; Welding Typical uses: Brake Lines; Power Steering Tube; Screw Lamp Bases; Condenser Plates; Condensers; Distiller Tubes; Evaporator Tubes; Evaporators; Ferrules; Heat Exchanger Tubes; Pressure Vessels; Pump Impellers for Oil Refining; Valve Bodies; Weld Torch Tips; Boat Hulls; Hot Water Tanks; Propeller Sleeves; Salt Water Baffles; Salt Water Piling Wrap; Salt Water Pipe Fittings; Salt Water Piping Systems; Ship Hulls; Tube Sheet for Salt Water Service; Water Hoses; Flanges Applicable Specifications: Bar – Rolled ASTM B122/B122M, ASTM B151/B151M, MILITARY MIL-C-15726; Condenser & Heat Exchanger Tube with Integral Fins – ASTM B956/B956M; Pipe – ASTM B466/B466M, ASTM B467, ASME SB467, ASME SB466; Plate – ASTM B432, Condenser Tube ASME SB171, MILITARY MIL-C-15726, ASTM B122/B122M, Condenser Tube SAE J463, Condenser Tube SAE J461, Condenser Tube ASTM B171/B171M; Rod – Welding AWS A5.15, ASTM B151/B151M, MILITARY MIL-C-15726; Sheet – SAE J461, MILITARY MIL-C-15726, SAE J463, ASTM B122/B122M; Strip – ASTM B122/B122M, MILITARY MIL-C-15726; Tube - Condenser Tube ASTM B552, Condenser Tube SAE J463, Condenser Tube ASME SB111, MILITARY MIL-T-22214, Condenser Tube MILITARY MIL-T-15005, Condenser Tube ASTM B111/B111M, ASTM B543/B543M, MILITARY MIL-T-16420, ASME SB543, MILITARY MIL-T-16420, ASME SB395, Condenser Tube SAE J461, ASTM B359/B359M, ASTM B469, ASME SB466, ASTM B466/B466M, ASME SB359, ASTM B395/B395M; Wire – MILITARY MIL-C-15726 |