MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger SPI
Syensqo (Solvay Specialty Polymers) Torlon® 4203 Polyamide-imide (PAI)  (discontinued **)
Categories: Polymer; Thermoplastic; Polyamide-imide (PAI); Polyamide-Imide, Extruded

Material Notes: Torlon 4203 is an unreinforced, lubricated, pigmented grade of polyamide-imide (PAI) resin for extrusion. It has the best impact resistance and greatest elongation of all the Torlon grades. Torlon PAI has the highest strength and stiffness of any thermoplastic up to 275°C (525°F). It has outstanding resistance to wear, creep, and chemicals. Torlon 4203 offers outstanding electrical properties, which makes it ideal for high performance parts such as connectors, switches and relays. In addition Torlon 4203 polyamide-imide can be used in applications such as thrust washers, spline liners, valve seats, bushings, bearings, wear rings, cams and other applications requiring strength at high temperature and resistance to wear. - High Flow: Torlon 4203 EXT - Higher Flow: Torlon 4203 HQ - Highest Flow: Torlon 4203 HHQ

Information provided by Solvay Specialty Polymers.

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Water Absorption, ASTM D570
  • Linear Mold Shrinkage, Flow, ASTM D955
  • Tensile Strength, ASTM D638, Type I
  • Tensile Stress, ASTM D1708
  • Elongation at Break, ASTM D638, Type I
  • Elongation at Break, ASTM D1708
  • Tensile Modulus, ASTM D638, Type I
  • Tensile Modulus, ASTM D1708
  • Flexural Strength, ASTM D790
  • Flexural Strength, ASTM D790
  • Flexural Modulus, ASTM D790
  • Flexural Modulus, ASTM D790
  • Compressive Strength, ASTM D695
  • Compressive Modulus, ASTM D695
  • Poissons Ratio, ASTM E132
  • Shear Modulus, Calculated
  • Izod Impact, Notched, ASTM D256
  • Izod Impact, Notched, ASTM D4812
  • Volume Resistivity, ASTM D257
  • Surface Resistance, ASTM D257
  • Dielectric Constant, ASTM D150
  • Dielectric Constant, ASTM D150
  • Dielectric Strength, ASTM D149
  • Dissipation Factor, ASTM D150
  • Dissipation Factor, ASTM D150
  • CTE, linear, ASTM D696
  • Thermal Conductivity, ASTM C177
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648, Unannealed
  • Rear Barrel Temperature
  • Nozzle Temperature
  • Mold Temperature
  • Drying Temperature
  • Dry Time
  • Moisture Content
  • Back Pressure
  • Screw Speed
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Solvay Specialty Polymers (includes former Solexis)

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.