MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
BASF Ultramid® 8231G HS 14% Glass Filled PA6 (Conditioned)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 10% Glass Fiber Filled

Material Notes: Ultramid 8231G HS is a heat stabilized, 14% glass fiber reinforced nylon 6 injection molding compound. It is also available in non-heat stabilized (Ultramid 8231) and/or pigmented versions. The glass fiber reinforcement enhances performance such as strength, stiffness and heat deflection temperature. The heat stabilizer system extends the properties at elevated temperatures. It also has excellent chemical resistance to greases, oils and hydrocarbons. njection molding compound possessing a balance of engineering properties combined with excellent processability and surface aesthetics.

Vendors:
Available Properties
  • Density, ISO 1183, dry
  • Melt Density, ISO 1183
  • Water Absorption, ISO Test, 24 hour
  • Water Absorption, ISO 62, beginning dry
  • Moisture Absorption at Equilibrium, ISO 62, beginning dry (23°C/50% R.H.)
  • Viscosity Measurement, Formic Acid
  • Linear Mold Shrinkage, ASTM Data; MD
  • Tensile Strength at Break, ASTM Test, 0.2 in/min
  • Tensile Strength at Break, ASTM Test
  • Tensile Strength at Break, ISO Data
  • Tensile Strength at Break, ASTM Test
  • Tensile Strength at Break, ISO Data
  • Tensile Strength at Break, ISO Data
  • Tensile Strength at Break, ASTM Test
  • Tensile Strength, Ultimate, ISO 527, 5mm/min
  • Elongation at Break, ISO 527, 5mm/min
  • Elongation at Break, ASTM Test, 0.2 in/min
  • Elongation at Break, ASTM Test
  • Elongation at Break, ISO Data
  • Elongation at Break, ISO Data
  • Elongation at Break, ASTM Test
  • Elongation at Break, ASTM Test
  • Elongation at Break, ISO Data
  • Tensile Modulus, ISO 527, 1mm/min
  • Tensile Modulus, ISO Data
  • Tensile Modulus, ISO Data
  • Tensile Modulus, ISO Data
  • Flexural Strength, ISO Data
  • Flexural Strength, ASTM Test
  • Flexural Strength, ASTM Test
  • Flexural Modulus, ISO Data
  • Flexural Modulus, ASTM Test
  • Comparative Tracking Index, IEC 60112
  • Specific Heat Capacity, Melt
  • Thermal Conductivity, Melt
  • Melting Point, 10 K/min
  • Melting Point, ASTM Test
  • Melt Temperature, Injection molding
  • Mold Temperature, Injection molding
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic
PA, Polyamide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.