| Hostacom TKC 420N C1 C15207 is a 10% talc filled PP copolymer, with good flowability, excellent impact/stiffness balance, very good scratch resistance and blooming resistance at elevated temperatures. Advanced technologies allowed for a significant reduction of mineral filler content which contributed to the reduction of final part weight. Product is available as a customized color matched, pellet form. This grade is delivered in C15207 color version. This grade is not intended for medical, pharmaceutical, food and drinking water applications. Availability: Asia-Pacific Application: Automotive Parts; Interior Trims Market: Automotive Attribute: Good Moldability; Non Blooming; Scratch Resistant Information provided by LyondellBasell. |