MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Ovako 100CrMo7-3 825Q Steel, Q/T (martensite)
Categories: Metal; Ferrous Metal; Alloy Steel; Low Alloy Steel; Carbon Steel; High Carbon Steel

Material Notes: General Information: Ovako 825 is a through hardening bearing steel that is mainly used for medium sized bearing rings, but it can also be used for machine components that require high tensile strength, hardness and toughness.
  • Through hardenability corresponding to a ring with approximately 30mm wall thickness (˜Ø50mm bar), quenched in oil
  • Suitable for martensitic or banitic hardening
  • Good machinability in soft annealed condition
  • Good dimensional stabilityBQ-Steel:
    825B – Standard825T - With a controlled low sulphur content to minimize the number of sulphide inclusions. Reduced carbon content and tighter chemical composition ranges

    IQ-Steel:825Q - Isotropic properties (IQ) and better fatigue strength due to higher cleanliness levels, and a finer size and distribution of non-metallic inclusions

    BQ-Steel:BQ-steel® is a bearing quality clean steel optimized for fatigue strength and is also ideal for new design solutions outside the bearing industry.

    IQ-Steel:IQ-Steel® is an isotropic quality ultra clean steel optimized for high fatigue strength under multi axial loading.

    Information provided by Ovako

  • Key Words: A485 (B6)
    Vendors:
    Available Properties
    • Density
    • Hardness, Rockwell C
    • Tensile Strength
    • Tensile Strength, Yield
    • Modulus of Elasticity
    • Poissons Ratio
    • Shear Modulus
    • Electrical Resistivity
    • CTE, linear
    • Specific Heat Capacity
    • Thermal Conductivity, Ambient temperature
    • Transformation Temperature, MS
    • Transformation Temperature, AC1
    • Transformation Temperature, AC3
    • Carbon, C
    • Chromium, Cr
    • Iron, Fe, As Balance
    • Manganese, Mn
    • Molybdenum, Mo
    • Nickel, Ni
    • Phosphorus, P
    • Silicon, Si
    • Sulfur, S
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    Manufacturer Notes:
    none

    Category Notes
    none

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

     

    Visit Zeus Inc. for PEEK Tubing
    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.