MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
UBE UPILEX 75S (75 micron) Polyimide Film
Categories: Polymer; Film; Thermoset; Polyimide, TS; Polyimide, Thermoset Film

Material Notes: Description: UPILEX, the ultra-high heat-resistant polyimide film, is the product of the polycondensation reaction between biphenyltetracarboxylic dianhydride (BPDA), of which process Ube Industries originally developed, and diamine. Most notable of these characteristics is UPILEX's physical, mechanical, electrical, and chemical properties under high-temperature conditions.

UPILEX-S demonstrates outstanding mechanical characteristics through a wide temperature range. UPILEX-S displays high tensile strength and modulus, and also features outstanding long-term heat resistance. Another advantage inherent in UPILEX-S is its high resistance to hydrolysis, as its properties are practically unaffected, even by immersion in boiling water for long periods of time.

Information provided by UBE.

Vendors:
Available Properties
  • Density, ASTM D1505
  • Film Tensile Strength at Yield, MD, ASTM D882, 200°C (Stress at 5% Elongation (MD))
  • Film Tensile Strength at Yield, MD, ASTM D882, 25°C (Stress at 5% Elongation (MD))
  • Film Elongation at Break, MD, ASTM D882, 25°C
  • Film Elongation at Break, MD, ASTM D882, 200°C
  • Flex Crack Resistance, ASTM D2176, Cycles Fold Endurance (MIT)
  • Secant Modulus, MD, ASTM D882, 200°C
  • Secant Modulus, MD, ASTM D882, 25°C
  • Coefficient of Friction, Dynamic, ASTM D1894, 25°C, film to film
  • Tear Strength Test, ASTM D1004, kg/mm, 25°C Tear Strength-Initiation [Graves] (MD)
  • Tear Strength Test, ASTM D1922, g/mm, 25°C, Tear Strength-Propagation [Elmendorf] (MD)
  • Film Tensile Strength at Break, MD, ASTM D882, 200°C
  • Film Tensile Strength at Break, MD, ASTM D882, 25°C
  • Volume Resistivity, ASTM D257, DC100V
  • Volume Resistivity, ASTM D257, DC100V
  • Surface Resistance, ASTM D257, DC100V
  • Surface Resistance, ASTM D257, DC100V
  • Dielectric Constant, ASTM D150
  • Dielectric Constant, ASTM D150
  • Dielectric Strength, ASTM D149, 50Hz, 75µm
  • Dielectric Strength, ASTM D149, 50Hz, 75µm
  • Dissipation Factor, ASTM D150
  • Dissipation Factor, ASTM D150
  • CTE, linear, Values determined by minute linear expansion tester at 5°C/min. temperature increments
  • Specific Heat Capacity, Differential Scanning Calorimeter
  • Thermal Conductivity, Laser Flash Method
  • Maximum Service Temperature, Air, Heat Treatment: 20,000 Hours
  • Glass Transition Temp, Tg
  • Flammability, UL94, VTM
  • Oxygen Index, JIS K7201
  • Shrinkage, JIS C2318
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.