MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Master Bond MasterSil 323S-LO Two Component, Silver Filled Silicone
Categories: Polymer; Thermoset; Silicone

Material Notes: Key Features:
  • Convenient handling
  • Addition cured system
  • Outstanding conductivity
  • NASA low outgassing
Product Description: Master Bond MasterSil 323S-LO is a two component, silver filled silicone with superb electrical conductivity along with very convenient processing. Both Parts A and B have smooth, paste consistency. The mix ratio is a user friendly 1 to 1 by weight. The working life for a 20 gram mass is 6 to 12 hours. The best cure schedule options are 8-12 hours at 130- 150°F, 4-6 hours at 160 to 180°F or 2-3 hours at 190 to 210°F. The system has low shrinkage upon curing and reasonably good dimensional stability for a silicone system. MasterSil 323S-LO has good adhesion to many materials including metals, ceramics, glass, composites as well as many types of rubber and plastics. Perhaps its most impressive feature is its flexibility and elongation. Consequently, it can withstand aggressive thermal cycling as well as mechanical and thermal shocks. Its paste consistency allows it to be easily applied as an adhesive, sealant or coating. Since it is an addition cured system it cures readily in thicknesses up to and beyond 1/4 inch thick. Both Parts A and B contain silver and appear that way in color. The service temperature range is -80°F to +400°F. MasterSil 323S-LO is most likely to be considered in aerospace, electronic, opto-electronic and specialty OEM applications, where excellent electrical conductivity, resounding flexibility, high temperature resistance and low outgassing, are necessary requirements.

Product Advantages:

  • Thick paste consistency
  • Long working life
  • Will cure in thicker sections
  • Superior conductivity
  • Vacuum compatible

Information provided by Master Bond, Inc.

Vendors:
Available Properties
  • Specific Gravity, Part B
  • Specific Gravity, Part A
  • Hardness, Shore A
  • Tensile Strength
  • Elongation at Break
  • Tensile Modulus
  • Adhesive Bond Strength, lap shear, aluminum to aluminum
  • Volume Resistivity
  • CTE, linear
  • Thermal Conductivity
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Shrinkage
  • Cure Time
  • Cure Time
  • Cure Time
  • Working Life, after mixing, 20 gram batch
  • Shelf Life, in original, unopened containers
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Master Bond Inc.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.