MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Online Metals
Visit Online Metals for fast service
on small quantity orders.
Michelman® DigiPrime® 5100 Primer  (discontinued **)
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: Primer for digital printing

Usage: DigiPrime® 5100 is a print primer which provides excellent adhesion of HP Indigo electro inks to treated films and paper. It adheres well to many synthetics, including soft vinyl. This product is designed for screen printing, but may also be applied via flexo and other methods.

Application data: DigiPrime® 5100 has been developed specifically for screen printing. It may also be applied via flexo, gravure, rod or roll coating systems. For screen printing, the following is recommended: 1. Mesh size: 180 lines per cm/460 lines per inch. 2. Thread diameter nominal: 27 micron 3. Squeegee: 80 Durometer A 4. Tension: 20-30N

Information provided by Michelman®

Vendors:
Available Properties
  • Specific Gravity
  • Volatiles
  • pH
  • Brookfield Viscosity, Spindle # 2, rpm 60
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.