MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
ArcelorMittal Ultragal® Z100 Zinc coatings and thin organic coating
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: Applications: With its ability to limit repeated waviness during deformation, combined with the proven qualities of Extragal®(surface quality, corrosion protection), Ultragal® is a coating specifically recommended for visible part applications in the automotive sector. With the Ultragal® production process, waviness in steel products can be controlled both before and after forming. In an optimized painting process configuration, Ultragal® lends the painted part very high-quality paint appearance (even better than a standard galvanized substrate). With waviness reduced to a very low value, Ultragal® also contributes to enhanced reproducibility of paint appearance quality.

Technical characteristics:

Surface appearance: The crystal structure of Ultragal® is not visible to the naked eye and the product offers optimum surface quality before and after painting. Control of the operating drive factors amplifying waviness at the secondary processing stage, in particular during drawing, further enhances paint appearance. We offer a waviness guarantee expressed as Wa 0.8 mm after drawing, which ensures product quality

Hardness: Ultragal® coating is relatively ductile, which reduces the risk of coating damage in the drawing tool.

Information provided by ArcelorMittal

Vendors:
Available Properties
  • Coating Weight, per side
  • Coating Weight, double-sided
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.