MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Metal adhesives
Master Bond EP30AN-1 Low Viscosity, NASA Low Outgassing Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive; Epoxy, Thermally Conductive

Material Notes: Key Features:
  • Thermally conductive
  • Electrically insulative
  • Low thermal expansion coefficient
  • NASA approved for low outgassing applications
  • Low viscosity with excellent flowability
  • Superior dimensional stability
Master Bond EP30AN-1 is a two part epoxy for high performance potting, sealing, coating and bonding featuring exceptionally high thermal conductivity, excellent electrical insulation properties and NASA low outgassing approval. It will cure at room temperature or more rapidly at elevated temperatures. Other attractive properties include superb dimensional stability and superior physical strength properties. Its low viscosity and excellent flow characteristics make it an ideal thermally conductive potting epoxy. EP30AN-1 is also an excellent adhesive/ sealant forming durable, rigid bonds that resist to thermal cycling and chemicals including water, oils, etc. over the wide temperature range of -60°F to +250°F. The coefficient of thermal expansion is desirably low. The color of Part A is gray and Part B is clear. Master Bond EP30AN-1 is widely used in applications where thermal conductivity, electrical isolation and low outgassing properties are required. It is particularly well suited to high vacuum environments.

Product Advantages:

  • Easy application: adhesive spreads or pours evenly and smoothly.
  • Versatile cure schedules: ambient temperature cures or fast elevated temperature cures as required.
  • High bond strength to a wide variety of substrates; excellent adhesive properties.
  • Exceptionally high thermal conductivity with excellent electrical insulation properties.
  • Good physical strength characteristics; especially high compressive strength.
  • Meets NASA low outgassing specifications

Information provided by Master Bond Inc.

Vendors:
Available Properties
  • Viscosity, Part B
  • Viscosity, Part A
  • Outgassing - Total Mass Loss, TML
  • Collected Volatile Condensable Material
  • Hardness, Shore D
  • Tensile Strength
  • Compressive Strength
  • Adhesive Bond Strength, Tensile lap, Aluminum to Aluminum
  • Volume Resistivity
  • Dielectric Constant
  • Dielectric Strength
  • CTE, linear
  • Thermal Conductivity
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Cure Time
  • Cure Time
  • Working Life, After mixing, 100 g batch
  • Shelf Life, in original, unopened containers
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Master Bond Inc.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Metal adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.