MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Daikin POLYFLON M-139 PTFE Molding Powder, Free Flow  (discontinued **)
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Molded

Material Notes: Free flow powder.

Processing Methods: Compression molding and automatic compression molding.

Features: Excellent fluidity. Apparent density is large and ideal for automated compression molding processes. Moldings have an excellent creep characteristic and post molding processability.

Information provided by Daikin Industries.

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Bulk Density, ASTM D894
  • Water Absorption, ASTM D570
  • Particle Size, Laser Method (Dry)
  • Viscosity, Melt viscosity
  • Linear Mold Shrinkage
  • Deformation, ASTM D621, 6.7 MPa load, at 100°C, 24 hrs
  • Deformation, ASTM D621, 13.7 MPa load, at 25°C, 24 hrs
  • Hardness, Shore D
  • Tensile Strength at Break, ASTM D638
  • Elongation at Break, ASTM D638
  • Tensile Modulus, ASTM D638
  • Flexural Modulus, ASTM D790
  • Compressive Strength, ASTM D695, 1% deformation
  • Izod Impact, Unnotched, ASTM D256
  • Coefficient of Friction, Non-lubricating
  • Coefficient of Friction, Lubricating
  • Coefficient of Friction, Static, Coated-steel surface
  • Taber Abrasion, mg/1000 Cycles, 9.8 N load, cs-10 wheel
  • Volume Resistivity, ASTM D257
  • Dielectric Constant, ASTM D150
  • Dielectric Constant, ASTM D150
  • Dielectric Strength, ASTM D149, Short time
  • Dissipation Factor, ASTM D150
  • Dissipation Factor, ASTM D150
  • CTE, linear, ASTM D696
  • Thermal Conductivity, ASTM C177
  • Melting Point
  • Maximum Service Temperature, Air, Continuous use
  • Flammability, UL94
  • Oxygen Index, ASTM D2863
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Daikin Industries

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.