MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Palm Labs Adhesives TURBO-LOCK SERIES 16 Anaerobic Thread Locking Compound
Categories: Polymer; Adhesive; Thermoset; Methacrylate; Methacrylate Adhesive

Material Notes: TURBO-LOCK SERIES 16 is a fast curing, GREEN, medium strength, wicking grade, anaerobic thread-locking compound for bonding and sealing threads, and pre-assembled parts. It is highly resistance to heat, vibrations, water, gases, oils, hydrocarbons and many chemicals. Disassembles with heat and hand tools.

Applications:

  • IPenetrates threads by capillary action. Medium strength thread-locker.
  • Ideal for sealing hairline cracks, small nuts and bolts.
  • Seals and welds porous metal parts. Localize heating and hand tools are needed for disassembly. Prevents corrosion and leakage.
  • Secure setscrews and other assemblies after settings are completed.
  • Fasteners on vibrating machines or moving components.
  • Meets Military specifications:MIL-S-46163 and MIL-S-22473

Part Numbers for this data: 16-001, 16-010, 16-050, 16-250, 16-1000

Information provided by Palm Laboratories Adhesives

Key Words: CAS No: 923-26-2, 15625-89-5, 80-15-9 and 114-83-0
Vendors:
Available Properties
  • Specific Gravity
  • Brookfield Viscosity, RVT Spindle 3 @ 20 rpm
  • Shear Strength, Compressive, Steel pins and collars, ISO 10123
  • CTE, linear, ASTM D696
  • Specific Heat Capacity
  • Thermal Conductivity, ASTM C177
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Cure Time, Handling
  • Cure Time, Functional
  • Cure Time, Full
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.