MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Chemically Resistant adhesives
3D Systems LaserForm® 17-4PH (A) H900 Stainless Steel Material
Categories: Metal; 3D Printing/Additive Manufacturing Metal; Ferrous Metal; Tool Steel

Material Notes: LaserForm 17-4PH (A) is fine-tuned for use with ProX® DMP 320 metal printer producing industrial parts with good corrosion resistance, high mechanical strength combined with excellent ductility. Mechanical properties of LaserForm 17-4PH (A) can be varied upon different heat treatments. LaserForm 17-4PH (A) is formulated and fine-tuned specifically for 3D Systems DMP 320 metal 3D printers to deliver high part quality and consistent properties.

LaserForm 17-4PH (A) is known for its outstanding combination of excellent corrosion resistance and high strength with good toughness. These good mechanical properties and corrosion resistance are maintained at temperatures up to 316°C (600°F). With these characteristics, LaserForm 17-4PH (A) is ideal for surgical instruments (sterilizable), aerospace, chemical, petrochemical and general metalworking applications.

Classification: The chemical composition of LaserForm 17-4PH (A) corresponds to a stainless steel 17-4 PH alloy according to ASTM F899, A564, A693 and UNS S17400 specifications.

Information provided by 3D Systems

Vendors:
Available Properties
  • Density, Absolute theoretical
  • Hardness, Rockwell C, ASTM E18
  • Tensile Strength, Ultimate, ASTM E8M, Vertical direction - Z
  • Tensile Strength, Ultimate, ASTM E8M, Horizontal direction - XY
  • Tensile Strength, Yield, ASTM E8M, Rp0.2%, Vertical direction - Z
  • Tensile Strength, Yield, ASTM E8M, Rp0.2%, Horizontal direction - XY
  • Elongation at Break, ASTM E8M, Horizontal direction - XY
  • Elongation at Break, ASTM E8M, Vertical direction - Z
  • Charpy Impact, ASTM E23, Notch
  • CTE, linear
  • Thermal Conductivity
  • Carbon, C
  • Chromium, Cr
  • Copper, Cu
  • Iron, Fe, Balance
  • Manganese, Mn
  • Nb + Ta
  • Nickel, Ni
  • Phosphorus, P
  • Silicon, Si
  • Sulfur, S
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
3D Systems Corporation

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Chemically Resistant adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.