MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
SEKISUI SPI KYDEX® 6513 Thermoplastic
Categories: Polymer; Thermoplastic

Material Notes: Integral "Frost" low heat release aviation sheet

KYDEX® 6513 is a proprietary, innovative, high performance thermoplastic sheet specifically formulated to meet the safety needs of the aviation industry while elevating aviation interior aesthetic. Color is filtered through frost-like finish to extend luxe design. Hues shift with movement of passenger or part, defining geometry and plane. KYDEX® 6513 is ideal to use with LED lighting, yet dynamic on its own.

KYDEX® 6513 meets all fire retardancy requirements set forth in Federal Aviation Regulations 25.853 paragraphs (a) and (d) (old (c)) including low heat release (65/65) in the OSU rate of heat release test. Its excellent properties make it the ideal material to form two and three-dimensional aircraft components.

Suggested Applications:

  • Seat parts
  • Armrests
  • Passenger service units
  • Kick panels
  • Bulkhead laminates
  • Life vest shrouds
  • Tray tables
  • Accent pieces
  • Window shades
  • Molding strips
  • Monitor shrouds

Features:

  • Available in P-3 texture and thicknesses from 0.71 mm (0.028 in) to 3.18 mm (0.125 in)
  • Meets the stringent requirements of FAR 25.853 paragraph (d) in all thicknesses and colors
  • Easy to fabricate with crisp detail, minimal rejects, and effect integrity
  • Can be formed on all standard presses and cut on all standard die-cutting machines
  • Easy to clean with aggressive cleaners and citrus-based cleaners (avoid ammoniated cleaners)
  • Secondary operations include: machining, sawing, blanking, punching, etc., are easily performed

Values based upon 3.18 mm (0.125 in) sheet unless otherwise specified

Information provided by Sekisui Polymer Innovations

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Moisture Absorption, ASTM D570
  • Hardness, Rockwell R, ASTM D785
  • Tensile Strength, ASTM D638
  • Tensile Modulus, ASTM D638
  • Flexural Strength, ASTM D790
  • Flexural Modulus, ASTM D790
  • Compressive Yield Strength, ASTM D695
  • Compressive Modulus, ASTM D695
  • Ultimate Bearing Strength, ASTM D953
  • Bearing Yield Strength, ASTM D953, 4% deflection
  • Shear Strength, ASTM D732
  • Dielectric Strength, ASTM D149, oil
  • CTE, linear, Transverse to Flow, ASTM D831
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648, Annealed
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.