MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Elkem (Bluestar Silicones) CAF® 731 Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Description: CAF 731 is a one component, thixotropic silicone elastomer, which cures at room temperature simply on contact with air moisture. It’s a product that is:
  • neutral : Alcohol type
  • Non flowing
  • White
  • Self-Adhesive (primerless)
Applications: CAF 731 is particularly suited for bonding, protection and maintenance applications. It is mainly attended as a flexible bonding and sealing agent between different types of materials substrate whose have different coefficients thermal of expansion, as glass, metal or plastic. It is recommended for:
  • Bonding/sealing in the aeronautic industry.
  • Elastic bonding or protection of electronic components.
  • Repair/servicing in industry and transport applications.
Advantages:
  • Its chemical neutrality guarantees no oxidation with metals principally used in electronic like copper.
  • Odourless, it is particularly well accepted in the workstation environment.
  • Outstanding adhesion on many substrates.
  • Good heat stability (-60°C - 180°C).
  • Outstanding mechanical properties.

Information provided by Bluestar Silicones

Vendors:
Available Properties
  • Specific Gravity
  • Storage Temperature
  • Hardness, Shore A, ASTM D2240
  • Tensile Strength, ASTM D412
  • Elongation at Break, ASTM D412
  • 100% Modulus, ASTM D412
  • Adhesive Bond Strength, Alu AG3, 1 mm thick joint, after 14 days curing NM748, 100% cohesive failure
  • Adhesive Bond Strength, PA 6.6, 30% fiber glass, 1 mm thick joint, after 14 days curing NM748, 100% cohesive failure
  • Tear Strength, ASTM D624
  • Maximum Service Temperature, Air
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Extrusion Rate, 3mm, 3bars, norm 495A
  • Cure Time, Skin formation
  • Cure Time
  • Cure Time
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.