| Temper: 1/2 Hard Fabrication Properties: Excellent Suitability – Soldering, Brazing, Capacity for Being Cold Worked; Good Suitability – Oxyacetylene Welding, Gas Shielded Arc Welding, Butt Weld; Fair Suitability – Capacity for Being Hot Formed Applicable Specifications: Bar – ASTM B591; Strip – ASTM B888/B88M, ASTM B591 |