Product Code: MSHQD-AC002-00 OT Chemical Name: 2,2’-dibenzothiazyl disulfide Trade Name: MBTS(DM) CAS No.: 120-78-5 Molecular Formula: C14H8N2S4 Typical Properties: Light yellow powder or granule, The relative density is 1.45~1.50. In room temperature, it slightly dissolved in benzene, toluene, carbon tetrachloride, trichlorobenzenes, acetone, ethanol, ethyl ether, and not dissolve in water, ethyl acetate, petrol and lye. Recommended Applications: It gives moderate processing safety and moderately fast cures with flat plateau. The vulcanizate characteristics are similar to those obtained with MBT. In fact, MBTS can often be used when MBT is too scorchy. Compounds cased on MBTS have slightly better aging and reversion resistance than corresponding ones based on sulfenamides. It can be boosted by use of secondary accelerators to achieve a faster cure and higher modulus. Information provided by Meyors Chemical INC Limited |