  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Tosoh OP-3HD High-density OP-3 grade, Fused Silica Glass
Categories: Ceramic; Glass

Material Notes: Tosoh OP-1 and OP-3 materials are manufactured by fusing a high-purity silica powder using Tosoh's proprietary oxy-hydrogen flame fusion process and a method of generating uniformly dispersed small bubbles inside the material. Thanks to its high purity and excellent infrared blocking properties, OP-1 has become the material of choice as a heat-insulating material for semiconductor and solar manufacturing equipment, such as epi and RTP chambers, and oxidation, diffusion, and CVD batch furnaces. OP-3 is an enhanced version of OP-1 material, with further reduced alkali content for use in processes that require extreme contamination control. OP-3HD is a high-density version of OP-3, with a smaller diameter bubble size distribution that provides enhanced sealing properties and lifetime for advanced batch furnace processes. Available in up to 1,000mm round and square ingots, OP-1, OP-3, and OP-3HD materials are 450mm wafer ready.

Information provided by Tosh Corporation

Vendors:
Available Properties
  • Density
  • Viscosity
  • Hardness, Vickers
  • Flexural Strength
  • Dielectric Constant
  • Dielectric Loss Index
  • CTE, linear
  • Specific Heat Capacity
  • Thermal Conductivity
  • Softening Point, (?=10^7.6)*2
  • Annealing Point, (?=10^13)
  • Strain Point, (?=10^14.5)
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.