MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Phillips Sumika Marlex® AHX-230 Polypropylene Impact Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Polypropylene Impact Copolymer, Heat Stabilized

Applications: Formulated for automotive interior trim, durables, housewares, and consumer products

Comments: Meets FDA Regulation 21 CFR 177.1520 and may be safely used as articles for use in contact with food except for articles used for packing or holding food during cooking. UL yellow card RTI of 65°C and a flame rating of UL94HB, these apply to natural color at a minimum thickness of 0.058".

The nominal properties reported herein are typical of the product but do not reflect normal testing variance and therefore should not be used for specification purposes.

Data provided by Phillips Sumika Polypropylene Company (PSPC).

Phillips Sumika Polypropylene Company has been shut down, as announced in 2011. This product had been discontinued prior to the shutdown announcement.

Vendors:
Available Properties
  • Density, ASTM D1505, injection molded specimen
  • Melt Flow, ASTM D1238
  • Hardness, Rockwell R, ASTM D785
  • Tensile Strength, Yield, ASTM D638, Type 1 Specimen, Rate: 2"/min; injection-molded specimen
  • Flexural Modulus, ASTM D790, Tangent; Rate 0.5"/min; injection-molded specimen
  • Izod Impact, Notched, ASTM D256, injection molded specimen
  • Izod Impact, Notched, ASTM D256, injection molded specimen
  • Impact Test, ASTM D3763
  • Maximum Service Temperature, Air, UL RTI 0.058 in. thickness, natural color
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648, injection molded specimen
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D256, injection molded specimen
  • Flammability, UL94, natural color
  • FDA, See notes for details.
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Phillips Sumika (Chevron Phillips Chemical Company)

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.