MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Metal adhesives
Permabond 731 Cyanoacrylate, toughened
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: PERMABOND® 731 is a toughened cyanoacrylate with very good impact and peel strength when compared to a conventional cyanoacrylate. It bonds rapidly at room temperature and its viscosity is stable over the shelf life of the product. This provides consistent performance. The product adheres to a variety of surfaces including steel, aluminum, galvanized steel, plastics and elastomers.

Features & Benefits:

  • Longer cure allows accurate alignment
  • Toughened and flexible
  • Ease of use – no mixing or heat cure
  • Bonds most materials
  • 100% reactive, no solvents

Information provided by Permabond.

Vendors:
Available Properties
  • Specific Gravity, Uncured
  • Viscosity, Uncured
  • Storage Temperature
  • Hardness, Shore D, ISO 868
  • Adhesive Bond Strength, ISO 4587, Acrylic, Shear
  • Adhesive Bond Strength, ISO 4587, PVC, Shear
  • Adhesive Bond Strength, ISO 4587, Zinc, Shear
  • Adhesive Bond Strength, ISO 4587, Aluminum, Shear
  • Adhesive Bond Strength, ISO 4587, Steel, Shear
  • Impact, ASTM D950, kJ/m2 Adhesive Impact Strength
  • Peel Strength, ASTM D903
  • Dielectric Constant
  • Dielectric Strength
  • CTE, linear
  • Thermal Conductivity
  • Cure Time, Buna N Rubber, handling time
  • Cure Time, Neoprene, handling time
  • Cure Time, Phenolic, handling time
  • Cure Time, Steel, handling time
  • Cure Time, ABS, handling time
  • Cure Time, Aluminum, handling time
  • Cure Time, full strength
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Metal adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.