| Polypropylene HJ45XI is clarified with the latest generation clarifier, taking advantage of its excellent aesthetics and processing efficiency. This product is a high-clarity PP grade for thin-walled packaging and injection molded containers for food and non-food applications. In addition to the excellent transparency level, this grade allows converters to achieve considerable energy and cost savings by processing the grades at lower temperatures and with shorter cycle times than similar products in the market HJ45XI is accompanied with. This grade possesses a high stiffness, which helps to improve top load properties as well as enable down gauging of the final product. Applications: Injection moulding, TWIM Information provided by Polychim Industrie. |