MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Azoty Tarnow™ Tarnamid® T-27 MW30 Polyamide 6 - Mineral Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Mineral Filled

Material Notes: 30% Mineral filled, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.

Tarnamid® has the following main properties:

  • High mechanical strength, rigidity and hardness
  • High impact strength
  • High vibration damping capacity
  • Good fatigue strength
  • Very good sliding properties, abrasion resistance, low coefficient of friction
  • High thermal resistance, admissible temperature of continuous operation from -60°C to +150°C
  • High chemical resistance, particularly to organic solvents, oils, lubricants and fuels
  • Considerable moisture absorption influencing mechanical and electrical properties
  • Self-extinguishing properties (fire retardant properties)
  • Good electro-insulating properties
  • Good optical properties, relatively good transparency of molded pieces with thickness below 3.2 mm made from natural Tarnamid® (not dyed and not compounded)
  • Can be used for the production of goods coming into contact with food (grades fulfilling requirement of European Union Directive No 2002/72/EEC) with latest amendments

Information provided by Azoty Tarnow™.

Vendors:
Available Properties
  • Specific Gravity, ISO 1183
  • Water Absorption, ISO 62
  • Linear Mold Shrinkage, Flow, ISO 294-4
  • Linear Mold Shrinkage, Transverse, ISO 294-4
  • Melt Flow, ISO 1133
  • Ball Indentation Hardness, ISO 2039-1
  • Tensile Strength, ISO 527
  • Elongation at Break, ISO 527
  • Tensile Modulus, ISO 527
  • Flexural Strength, ISO 178, 3.5% flexure
  • Flexural Modulus, ISO 178
  • Charpy Impact Unnotched, ISO 179 1eU
  • Charpy Impact, Notched, ISO 179 1eA
  • Volume Resistivity, IEC 93
  • Surface Resistance, IEC 93
  • Dielectric Strength, IEC 243-1
  • Comparative Tracking Index, IEC 112
  • Melting Point
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75
  • Vicat Softening Point, ISO 306
  • Minimum Service Temperature, Air
  • Flammability, UL94
  • Glow Wire Flammability Index, PN-EN-60695-2-12
  • Melt Temperature
  • Mold Temperature, 80 - 90°C is recommended
  • Drying Temperature
  • Moisture Content
  • Injection Pressure, 80 MPa is recommended
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Azoty Tarnow™ (Zaklady Azotowe)

Category Notes
Plastic
PA, Polyamide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.