MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Carlson C 800 Nickel-Iron-Chromium Alloy
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy

Material Notes: General Description

Carlson Alloy C 800 is a nickel-iron-chromium alloy, combining high strength with excellent resistance to oxidation and carburization at elevated temperatures. This alloy resists sulfur attack, internal oxidation, scaling and corrosion in a wide variety of industrial atmospheres.

The high chromium content of C 800 assures good resistance to oxidation, while the nickel content imparts a fair degree of resistance to stress corrosion cracking.

Carlson Alloy C 800H is essentially the same alloy as C 800 except the carbon content is restricted to the upper portion of the specified range. C 800H also receives a solution-anneal which produces a coarser grain structure. This assures higher creep and rupture strengths, enabling C 800H to be used in applications that require prolonged exposure at elevated temperatures and/or in corrosive environments.

Applications

  • Chemical Processing – heat exchangers for nitric acid production; calciners, dryers and recuperators in soda ash plants; process equipment in fiberglass and ore processing plants.
  • Petroleum and Petrochemical – tubing for hydrotreaters and effluent coolers; tubing, manifolds, pigtails and quench lines in hydrogen reformers; flare tips for incinerating waste gasses in refineries; reformer tubing, catalyst grid supports and converters for ammonia production; ethylene furnaces; tubing, bends and flanges for vinyl chloride production; steam superheaters for styrene production.
  • Power Generation – boiler superheaters and reheater tubes and shields; gas turbine combustion cans, transition liners and diffusers.
  • Thermal Processing – baskets and boxes, fixtures and radiant tubes for heat treat furnaces.
  • Steel Production – coke plat quench-car liners and process piping; steam methane reformers and recuperators for direct reduction of iron ore.

Information provided by Carlson

Key Words: UNS N08800
Vendors:
Available Properties
  • Density
  • Tensile Strength at Break
  • Tensile Strength, Yield
  • Elongation at Break
  • Modulus of Elasticity
  • Modulus of Elasticity
  • Modulus of Elasticity
  • Magnetic Permeability, 200 Oersted
  • Curie Temperature
  • CTE, linear
  • Melting Point
  • Solidus
  • Liquidus
  • Aluminum, Al
  • Carbon, C
  • Chromium, Cr
  • Copper, Cu
  • Iron, Fe
  • Manganese, Mn
  • Nickel, Ni
  • Silicon, Si
  • Sulfur, S
  • Titanium, Ti
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.