MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Trinseo Magnum™ 3416 SC Natural Plus ABS Resin
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: MAGNUM™ 3416 SC is the reference high-heat ABS in the automotive industry. It is universally suitable for all interior and exterior applications. It is approved at all major OEMs. MAGNUM™ 3416 SC is globally available, locally produced in major car production regions.

Benefits:

  • Lot to lot consistency allowing for optimal machine parameters setting from the start
  • Self-coloring enabling improvement of costs by using less pigments and lowering your logistic costs
  • Low VOC allowing to better interior air quality facing increasing regulatory and OMEs constraints
  • Heat stability during wide range of processing temperatures: enhanced part design freedom
Application:
  • Main interior and exterior automotive applications
  • Mid-consoles
  • Door panels
  • Door handles
  • Pillars
Automotive Specifications:
  • BMW GS 93016 Color: Natural
  • FORD WSS-M4D690-B1
  • JLR STJLR.51.353
  • JLR STJLR.51.5262 Color: Natural
  • PSA Peugeot-Citroen ABS-0021
  • VAG VW-TL 527 A
  • DAIMLER DBL 5404.04
  • GM GMW15572P-ABS-T2 Color: Natural
  • JLR STJLR.51.5229
  • PSA Peugeot-Citroen ABS-0019
  • RNPO AS32-1
  • VAG VW-TL 527 B

Information provided by Dow

This product line was spun off from Dow Chemical to Styron in 2010.

Vendors:
Available Properties
  • Bulk Density, ISO 60
  • Density, ISO 1183B
  • Melt Flow, ISO 1133
  • Tensile Strength, Yield, ISO 527-2
  • Elongation at Yield, ISO 527-2
  • Tensile Modulus, ISO 527-2
  • Flexural Strength, ISO 178
  • Flexural Modulus, ISO 178, 3 points
  • Charpy Impact, Notched, ISO 179/1eA
  • Charpy Impact, Notched, ISO 179/1eA
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75-A, Unannealed
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75-A, Annealed
  • Vicat Softening Point, ISO 306-B
  • Flame Spread, ISO 3795, 2 mm
  • Flammability Test
  • Flammability Test
  • Shrinkage, ISO 294-4
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Trinseo, former Styron

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.