| Duroxite 100 Pipe is manufactured by depositing chromium-rich, abrasion-resistant materials on a mild steel base using a traditional arc welding process. The hardfacing overlay pipe is designed with extreme wear capabilities for working in the most severe environments. Duroxite 100 Pipe is available with double or multiple overlay passes. Schedule 40 and Schedule 80 steel pipe as well as tubing can be hardfaced. Overlay Pipe can be fabricated as square-to-round transitions, elbows, T or Y-shaped, or as long sweeps. Key Benefits - Same wear resistance guaranteed from surface down to 75% of the overlay
- Optimal carbide composition to provide good combination of wear resistance and homogenous bonding
Typical Applications: Duroxite 100 Pipe is widely used in the mining, cement, oil sands, dredging, recycling and steel production industries. Some specific applications include:- Mining, Cement, Oil Sands: Slurry pumps, chutes
- Dredging: Dredging pipes
- Recycling: Cullet glass
- Steel: Air ducts, carbon injection pipes, suction lines, troughs
Data provided by SSAB. |