MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Specialty Compounds RTP Company
ITW Densit® Ducorit® A2G Grout
Categories: Ceramic

Material Notes: Ducorit® R and A product lines are based on innovative ultra high performance cementitious technology that was developed in house by Densit® for use in structural grouted connections for wind turbine foundations and concrete tower joints. UHPC and HPC Densit® Technology. The differentproperties of Ducorit® A2G and Ducorit® R5G are obtained by a unique mix of high quality cement, aggregates and additives. The products are manufactured as ready-to-mix grout, in 25 kg to 1000 kg bags. Ducorit® products are characterized by extreme strength and high stiffness making Ducorit® a strong structural component, meeting international high design standards.

Information provided by ITW Performance Polymers.

Vendors:
Available Properties
  • Grain Size
  • Flexural Strength, EN- 196-1, 28 days @ 20°C
  • Compressive Strength, 24 hrs
  • Compressive Strength, 7 days
  • Compressive Strength, 28 days
  • Compressive Strength, 91 days
  • Shrinkage, es,m,91. SKVM II
  • Shrinkage, es,i,91. SKVM II
  • Shelf Life, dry and RH<70%
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Master Bond adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.