MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Geon® Performance Solutions 210 Series 217 Blending Resin Polyvinyl Chloride Homopolymer (PVC Homopolymer)
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: Geon® 217 is a low to medium molecular weight homopolymer blending resin intended for use as a formulation tool in plastisol formulations.It improves air release performance resulting in reduced scrap rates. It decreases high shear viscosity providing an improved 'ease of coating' performance resulting in a more uniform plastisol coating and improving line up time. It reduces viscosity aging characteristics, providing increased plastisol usage (pot life). It reduces surface gloss of films or coated products resulting in less surface blocking and improved handling. Geon® 217 is recommended for solid and foamed plastisol applications such as coated fabric, cast films and coatings, foam mats and pads.

Typical values. This resin is shipped in multi-wall paper bags. Geon® ALTC (formulation): 60phr Geon® 121A, 40phr Geon® 217, 57phr DINP, 3phr ESO, and 2phr Therm-Chek SP 120 LOHF Geon® STP 1203(formulation): 60phr Geon® 178, 40phr Geon® 217,and 60phr DOP

Geon Performance Solutions was created from PolyOne in 2019.

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Volatiles, Internal Method, Geon® STP 1242
  • Apparent Bulk Density, Internal Method, Geon® STP 1169
  • Particle Size, Internal Method, Geon® DFT 1466
  • Particle Size, Internal Method, 94.2%; Geon® DFT 1466
  • Particle Size, Internal Method, 99%; Geon® DFT 1466
  • Relative Viscosity, Internal Method, Cyclohexanone 1%
  • Brookfield Viscosity, Internal Method, One Day Viscosity @ 2rpm Geon® ALTC 22 (with provided formulation)
  • Brookfield Viscosity, Internal Method, Initial Viscosity @ 2rpm Geon® ALTC 22 (with provided formulation)
  • Brookfield Viscosity, Internal Method, Initial Viscosity @ 20 rpm; Geon® ALTC 22 (with provided formulation)
  • Brookfield Viscosity, Internal Method, One Day Viscosity @ 20rpm Geon® ALTC 22 (with provided formulation)
  • Viscosity Measurement, ASTM D1243-60-A, Inherent
  • Melt Flow, Internal Method, Severs Efflux; Geon® ALTC 23 (with provided formulation)
  • Haze, Internal Method, Fused 5 mins Geon® ALTC 66 (with provided formulation)
  • Gloss, Internal Method, 60° Fused 5 mins Geon® ALTC 65 (with provided formulation)
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.