MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Synthos Surpren™ H-4535 / M-4035 Chlorosulfonated Polyethylene
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: General introduction: Chlorosulfonated polyethylene, referred to as CSM, is a kind of elastomer which has completely saturated main chain and pendant group and can be vulcanized by all kind of cross linking agent. Because of its unique molecular structure, CSM vulcanizate has excellent ozone resistance and weatherability. In additional, properly formulated CSM vulcanizate has excellent resistance to heat, oil, chemicals and aging. SUNPREN™ CSM is chlorosulfonated polyethylene produced by Sundow Polymers Co., LTD.

Characteristic of CSM:

  • Permanent bright colors
  • Superior ozone and weather resistance, even for the formation without carbon black
  • High working temperature up to 150?
  • Resistance to a wide range of aggressive chemicals
  • Moderate resistance to oil and solvent depending on chlorine level
  • Good flame retardancy
  • Electrical insulating properties
  • Excellent resistance to abrasion and mechanic abuse
Distinguishing Features:
  • General –purpose grade
  • Good balance in physical properties and processability
Application: Automotive hoses, rubber seal, wire and cable,rubber rollers,tape and specialty rubber products

Information provided by Sundow Polymers Co., Ltd

Vendors:
Available Properties
  • Mooney Viscosity, ML(1+4)
  • Chlorine, Cl
  • Sulfur, S
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.