| SI 120 is a surface insensitive cyanoacrylate adhesive that is used in applications that require faster cure speeds, on parts that are dry, and on parts that may be acidic. The SI Series bonds a wide range of similar and dissimilar surfaces. Substrates bonded include ABS, Acrylic, Aluminum, Bakelite, Brass, Chloroprene, Chrome, Cooper, EPDM, Fiberglass, Latex, Leather, Natural Rubber, NBR, Neoprene, Nitrile, Nylon, Phenolic, Polycarbonate, Polyester, Polystyrene, Porcelain, PVC, SBR, Steel, Valox, and Wood. Information provided by Adhesive Systems, Inc. |