MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Elkem (Bluestar Silicones) SILBIONE® LSR 4755 Liquid Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Liquid Silicone Rubber (LSR)

Material Notes: Description: SILBIONE® LSR 4755 is a self-bleeding healthcare grade liquid silicone rubber that creates a lubricious surface on the molded part after vulcanization.

Applications:

  • Molded medical applications for skin contact or <30 day implantation
  • General molded parts where high slip is required
  • Needleless valves
  • O-rings
  • Stoppers
  • Seals
  • Balloons
Features:
  • High slip surface
  • Long bleed life that helps prevent slit healing
  • Delayed bleed to prevent mold fouling
  • High clarity
  • Excellent mold release for shorter cycle times
  • Rapid cure at elevated temperatures
  • No post cure is needed
  • Customizable in a range of durometers and load levels to meet specific performance requirements

Information provided by Bluestar Silicones

Vendors:
Available Properties
  • Specific Gravity, TP 013
  • Storage Temperature
  • Hardness, Shore A, ASTM D2240, Press Cured, 5 min, 177°C
  • Tensile Strength, ASTM D412, Press Cured, 5 min, 177°C
  • Elongation at Break, ASTM D412, Press Cured, 5 min, 177°C
  • Tear Strength, ASTM D624, Die B, Press Cured, 5 min, 177°C
  • Compression Set, ASTM D395-98, Method B, Press Cured, 5 min, 177°C
  • Extrusion Rate, TP 031
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.