MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Dow Dow™ 5004I LDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Extrusion Grade

Material Notes: Product Description: Dow LDPE 5004I is used for fresh milk cartons, liquid/juice containers, dry foods packaging, snack foods packaging, moist foods packaging, and medical packaging. Dow LDPE extrusion coating resins provide optimal neck-in and draw-down performance with minimal taste/odor contribution.
  • A low melt index coating resin for demanding packaging applications

Complies with: US FDA 21 CFR 177.1520©2.2a; US FDA DMF; Canadian HPFB No Objection (With Limitations); EU No 10/2011; Japan Hygienic Olefin and Styrene Plastics Association. Consult the regulations for complete details.

Availability: Asia Pacific; Latin America; North America

Additive: Antiblock: No; Processing Aid: No; Slip: No

Agency Ratings: DMF; FDA 21 CFR 177.1520©2.2; EU No 10/2011; Canadian HPFB No Objection (With Limitations); JHOSPA

Form: Pellets

Processing Method: Cast Film; Extrusion Coating

Information provided by The Dow Chemical Company

Vendors:
Available Properties
  • Density, ASTM D792
  • Water Vapor Transmission, ASTM F1249, 1.0 mil, Extrusion Coating
  • Melt Flow, ASTM D1238
  • Neck In, 1.0 mil
  • Coating Weight
  • Film Tensile Strength at Yield, MD, ASTM D882, Cast Film
  • Film Tensile Strength at Yield, TD, ASTM D882, Cast Film
  • Film Elongation at Break, MD, ASTM D882, Cast Film
  • Film Elongation at Break, TD, ASTM D882, Cast Film
  • Coefficient of Friction, Dynamic, ASTM D1894, vs. Itself
  • Elmendorf Tear Strength MD, ASTM D1922, Cast Film
  • Elmendorf Tear Strength TD, ASTM D1922, Cast Film
  • Dart Drop Test, ASTM D1709A, Cast Film
  • Film Tensile Strength at Break, MD, ASTM D882, Cast Film
  • Film Tensile Strength at Break, TD, ASTM D882, Cast Film
  • Heat Seal Strength Initiation Temperature, 1.0 mil, Extrusion Coating
  • Melting Point
  • Vicat Softening Point, ASTM D1525
  • Haze, ASTM D1003, Cast Film
  • Gloss, ASTM D2457, 45°, Cast Film
  • Melt Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Dow Chemical

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.