MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Vitro Minerals LA 400 Recycled Glass Powder
Categories: Ceramic; Glass

Material Notes: LA Glass powders are functional fillers and extenders produced from clean, post-industrial, glass feedstocks. X-ray diffraction and scanning electron microscopy confirms that the LA Glass calcium aluminosilicate powders are fully amorphous and contain no crystalline silica. The glass chemistry results in relative chemical inertness, making LA Glass resistant to blooming, blistering, or chemical degradation in harsh environments. LA Glass powders enhance a wide range of paints, coatings, plastics, and adhesives. High consistent brightness, tint retention and stain/scrub resistance can be achieved in most paint and coating systems. LA Glass powders have low oil absorption and can be easily dispersed in water- or solvent-based systems. The feedstocks are certified post-industrial and are free from contaminants associated with post-consumer curbside glass. Vitro Minerals’ processing system and true particle size classification provides consistent product quality for 7 grades (LA-300, LA-350, LA-400, LA-500, LA-600, LA-700, LA-800) with finenesses and brightness covering a range of potential applications. Under a microscope, LA Glass powder particles are transparent, angular-shaped particles with similar dimensions in the x, y and z axis.

Information provided by Vitro Minerals.

Vendors:
Available Properties
  • Specific Gravity, ASTM D153
  • Bulk Density, ASTM C110
  • Brightness, Y value
  • Oil Absorption, ASTM D281
  • Moisture Absorption at Equilibrium, ASMT C566, Free
  • Particle Size, Laser interferometer, d50 median
  • Particle Size, Laser interferometer, d98 top
  • Particle Mesh Size, ASTM C25, 99.9%
  • pH, AFS 113-87-S
  • Hardness, Mohs
  • Surface Resistance, ASTM D2448
  • Refractive Index, ASTM D801
  • Al2O3
  • B2O3
  • CaO
  • Fe2O3
  • Loss on Ignition(%)
  • MgO
  • Na2O or K2O
  • SiO2
  • TiO2
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.