| Temper: As Permanent Mold Cast Casting Characteristics: High – Effect of Section Size; Medium – Fluidity, Casting Yield, Gassing; Low - Drossing, Shrinkage in Solidification Fabrication Properties: Excellent Suitability – Soldering, Brazing Typical uses: Ornamental Castings; Cooling Equipment; Heating Equipment; Nuts; Bearings; Bushings; Cryogenic Valves; Fittings Used to 550 F; Gears; Medium Pressure Hydraulic Equipment; Piston Rings; Pump Impellers; Pumps Used to 550 F; Valve Components; Valves for Water Meters; Marine Castings; Medium Pressure Steam Equipment to 550 F Applicable Specifications: As Centrifugal Cast – Castings ASTM B271/B271M, Castings SAE J461, Castings SAE J462; As Continuous Cast – Castings SAE J462, Castings SAE J461, Castings ASTM B505/B505M; As Sand Cast – Castings SAE J462, Castings SAE J461, Castings ASTM B584, Castings ASTM B61, Castings ASME SB584, Castings ASME SB61; Fitting – ASME SB61, ASTM B61, FEDERAL WW-P-460, ASME B16.24; Flanges ASTM B61, ASME SB61, FEDERAL WW-P-460; Ingot - ASTM B30; Valves MILITARY MIL-V-17547 |