MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Avient Teslart™ Powder Polyaniline chains grafted to lignosulfonic acid  (discontinued **)
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoplastic

Material Notes:

Description/Features:

  • An inherently conductive polymer consisting of polyaniline chains grafted to lignosulfonic acid
  • polymerized in an aqueous solution into the form of a wet cake, or dried into a powder form
  • conductivity levels are controlled during the polymerization process
  • exhibiting redox activity, highly dispersible and cross-linkable properties.

Applications:

  • Anti-fouling Marine Coatings
  • Batteries
  • Antistatic Fabrics, Coatings and Packaging
  • Coil coating
  • Conductive Inks and Adhesives
  • Corrosion resistant coatings
  • EMI/RFI Shielding
  • Radar / Microwave Absorption and Sensors

Processing Method:

  • Can be processed with normal dispersing equipment, such as high speed dispersers
  • for optimal results, contact PolyOne's technical staff to determine recommended processing.

Easier to process and more environmentally friendly, Teslart ICPs replace traditional materials in applications where it is challenging to use traditional fillers such as carbon-black, salts or metal fillers. Tunable surface resistivity values are achievable with Teslart ICPs.

Disclaimer: Material should remain sealed in storage. Avoid freezing.
Teslart ICP's are made under license of NASA's U.S. Patent Nos. 5,968,417; 6,059,999; 6,299,800 and other patents pending.

Information provided by PolyOne Corporation.

Vendors:
Available Properties
  • Specific Gravity, Calculated
  • Solids Content
  • Particle Size
  • pH
  • pH, Cyclic Voltammetry, Redox range (pH)
  • Electrical Resistivity, 4 Point Probe
  • Surface Resistivity per Square, 4 Point Probe
  • Decomposition Temperature, Heat Stability
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Avient, former PolyOne Corporation

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.