MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Aremco
Aremco Ceramacast™ 905 Silicone-Ceramic Potting Compound
Categories: Ceramic; Oxide; Silicon Oxide; Polymer; Thermoset; Silicone

Material Notes: Ceramacast™ 905 is a silicone-bonded, ceramic filled high temperature adhesive and potting compound. Two-component (liquid + powder), Moisture Resistant Silicone, Coarse Grain Compound.

Cure:
Step 1. Dry for 24 hours room temperature to allow solvent to evaporate.
Step 2. Bake at 150 ºF for 1 hour.
Step 3. Bake at 250 ºF for 1 hour.
Step 4. Bake at 350 ºF for 1 hour.
Step 5. Final cure at 450 ºF for 1 hour.

Vendors:
Available Properties
  • Density, Liquid
  • Density, Powder
  • Porosity, after 900°F
  • Volume Resistivity
  • Dielectric Strength
  • CTE, linear
  • Maximum Service Temperature, Air
  • Shrinkage
  • Cure Time
  • Cure Time
  • Shelf Life, Liquid
  • Shelf Life, Powder
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.