MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Paratherm Corporation Paratherm™ MR Heat Transfer Fluid
Categories: Fluid

Material Notes: Description: Paratherm MR® is a mid-range heat transfer fluid. It is efficient across the temperature range, thermally stable and cost-effective. Non-aromatic and non-toxic, the fluid is safe to use and is easy to dispose. Used or contaminated fluid can be safely combined with spent lubricating oils and recycled locally. It is designed for a broad variety of applications such as batch reactors, laminating lines and plastics mold tenoerature control.

Information provided by Paratherm Corporation.

Vendors:
Available Properties
  • Density
  • Molecular Weight, ASTM D2502, average
  • Heat of Vaporization, calculated
  • CTE, linear
  • Boiling Point, ASTM D1160, Range, 10% fraction to 90% fraction
  • Maximum Service Temperature, Air, optimum use range
  • Maximum Service Temperature, Air, max. recommended film temperature
  • Minimum Service Temperature, Air, optimum use range
  • Pour Point, ASTM D97
  • Flash Point, ASTM D92, coc
  • Ignition Temperature, ASTM E659, Autoignition
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.