MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
SSAB Duroxite® 200 Wire Welding Wire
Categories: Metal; Ferrous Metal

Material Notes: Duroxite 200 Wire is a flux-cored welding wire for hardfacing components subject to severe abrasive wear and moderate impact applications using an open-arc welding process. The deposit contains hard complex carbides in a tough matrix and performs exceptionally well for both fine and coarse abrasion applications. It naturally reveals stress-relief cracks after welding. Duroxite 200 Wire is suitable for single or double-layer deposits. Preheating, interpass temperature, and post-weld heat treatment are as needed according to base metal recommendations. If welding with downhill or uphill position, reduced wire feed speed and voltage are preferred to apply.

Key Benefits

  • Same wear resistance guaranteed from surface through 75% depth of overlay in multi-layer deposit.
  • Optimal alloy formulation that forms a primary chromium-rich carbide with co-existing refined multi-alloys carbides which provide a good combination of wear and impact resistance.
Typical Applications: Duroxite 200 Wire is mainly designed to use for hardfacing components undergoing heavy wear by earth, sand or abrasives up to 600 ºC (1100ºF). Typical examples include: Sand and earthmoving equipment, ground engaged teeth, slurry pipe, railway ballast tampers, dredge buckets and lips, sand dreging parts, dragline bucket liners, crushing equipment, brick industry components, coke hammers, rippers, sizing screens, Muller tires, catalyst lift pipes, pump impellers, fan blades, rockwool rolls, wear plates or wear parts operating at high temperature in steelmaking industry.

Data provided by SSAB.

Vendors:
Available Properties
  • Hardness, Rockwell C, Single pass
  • Hardness, Rockwell C, Double pass
  • Hardness, Rockwell C, Multiple passes, 3-layer deposit on mild steel
  • Carbon, C
  • Carbon, C
  • Carbon, C
  • Chromium, Cr
  • Chromium, Cr
  • Chromium, Cr
  • Iron, Fe, Balance
  • Iron, Fe, Balance
  • Iron, Fe, Balance
  • Manganese, Mn
  • Manganese, Mn
  • Manganese, Mn
  • Silicon, Si
  • Silicon, Si
  • Silicon, Si
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
SSAB Tunnplat AB

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.