MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Dow Bynel® E418 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade

Material Notes: Bynel® Series 3800 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene (PE) resins.

Applications: Bynel® 3810 and Bynel® 3859 adhere to a wide variety of materials. They are most often used to adhere to PE, PS, and EVOH. They can also be used to adhere to polyamide. They provide outstanding adhesion to PS. They are typically used to bond PS to EVOH barrier resins in opaque thermoformed container applications. They are also well suited to structures such as PS/Bynel® /EVOH/Bynel® /PE, because they adhere to polyolefins in addition to PS and EVOH. The primary difference between Bynel® 3810 and Bynel® 3859 is their rheology. Bynel® 3810 and Bynel® 3859 can be used in coextrusion processes including: cast film/sheet blown film Bynel® 3860 and Bynel® 3861 are most often used to adhere to PE, ionomer, PS, EVOH, and PET. They can also be used to bond to PP, PVC, PVDC, PC, and polyamide. Bynel® 3860 and Bynel® 3861 are used in transparent PS/EVOH/PE structures as well as PET/PE cast sheet. Bynel® 3860 is used to coextrusion coat EVOH onto OPP. The primary difference between Bynel® 3860 and Bynel® 3861 is their rheology. Bynel® 3860 and Bynel® 3861 can be used in coextrusion processes including: cast film/sheet blown film extrusion coating Bynel® E418 provides good adhesion to unprimed oriented polyester film. It will also adhere to PE, EVA, Surlyn® , EVOH, PET, PC, PS, polyamide, PVC, and PVDC. Bynel® E418 will also bond to fabric and nonwovens.

Physical properties of Bynel® 3800 Series resins are typical of EVA resins with similar density and melt index values. The rheology characteristics of each grade are different, so one may be better suited than the others to a particular extrusion process.

Information provided by DuPont Packaging Polymers.

This former DuPont product line is now a Dow product line.

Vendors:
Available Properties
  • Density, ASTM D792
  • Viscosity, estimated from log-log graph
  • Melt Flow, ASTM D1238
  • Melting Point, Freezing point via DSC/ASTM D3418
  • Melting Point, Melting point via DSC/ASTM D3418
  • Vicat Softening Point, ASTM D1525
  • Processing Temperature, Extruder forward zone and adapter. Degrades above 238°C.
  • Nozzle Temperature, Die
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Dow Chemical (former DuPont)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.