MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Evonik Protectosil® CTI Surface Treatment
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: A surface-applied clear liquid that penetrates concrete and provides an organofunctional molecule to inhibit the electrochemical corrosion process between the rebar and the chloride ions, and oxygen and moisture within the concrete.
Protectosil CIT:
  • Dramatically reduces the chloride-ion-induced corrosion rate of concrete steel reinforcement
  • Reduces corrosion in carbonated concrete steel reinforced structures
  • Is an easy-to-use treatment that penetrates the concrete and chemically bonds with steel, cement paste and other siliceous material
  • Will not discolor or change the substrate’s surface appearance or surface friction
  • Effectively inhibits macrocell (mat-to-mat) and microcell (along rebar) corrosion of steel-reinforced concrete
  • Mitigates corrosion of rebar even in structures subjected to an environment with high relative humidity
  • Repels additional water and chloride ions
APPROPRIATE APPLICATIONS:
  • Steel-reinforced cast-in-place, precast, post tension, GFRC, prestressed or other steel-reinforced concrete
  • Parking decks, facades, balconies, walkways, piers, bridge decks, beams, columns and other steel-reinforced concrete structures
  • Marine environments with high relative humidity and areas where deicer salts are used
ADVANTAGES: Protectosil CIT dramatically decreases both mat-to-mat (>90%) and microcell (>87%) corrosion currents. Protectosil CIT works on the molecular level to effectively inhibit the electrochemical interaction of the corrosion process. This advanced inhibiting action makes Protectosil CIT the best choice for difficult applications. Applied to concrete structures repaired with polymer concrete, Protectosil CIT can equalize the differences in electrochemical potential between the polymer concrete and the existing concrete. The product:
  • Inhibits corrosion of carbon and galvanized steel rebar
  • Is effective in both marine and high-humidity environments
  • Is easy to apply
  • Is effective in heavily chloride-contaminated concrete
  • Is effective in carbonated concrete
  • Complies with VOC regulations
  • Is vapor permeable
  • Dries quickly
  • Prevents ingress of additional chlorides

Information provided by Evonik

Vendors:
Available Properties
  • Density
  • Volatile Organic Compounds (VOC) Content
  • pH
  • Viscosity
  • Flash Point
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Evonik Corporation (Former Evonik Degussa GmbH)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.