MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Unifrax Insulfrax® 1100C Modules
Categories: Ceramic

Material Notes: Insulfrax® 1100C Modules are a family of high-temperature module products based on Unifrax's Anchor-Loc® attachment systems. Modules used in the Anchor-Loc® systems are constructed with Insulfrax S Blanket. Each type of Insulfrax 1100C Module can be easily fastened to interior steel shells of all types of heat processing equipment with several different attachment systems.

Insulfrax S Blanket, which is utilized in Insulfrax 1100C Modules, is based on a calcium, magnesium, silicate chemistry to provide thermal insulation at recommended operating temperatures up to 2012°F (1100°C); Insulfrax products also meet European regulatory requirements (Directive 97/69/EC).

Insulfrax 1100C Modules are fabricated from eight folds of one-inch thick Insulfrax S Blanket to achieve precompression of the block during manufacture. The folded blanket layers are secured to the metallic module anchor by two alloy tubes. Flanges on the end of the tubes effectively lock the position of the tubes relative to the anchor at the time of installation.

    Application
  • Annealing furnace linings
  • Slow cool covers for slabs and ingots
  • Process heater linings
  • Aluminum homogenizing furnace linings
  • Aluminum ladle covers
  • Personnel heat shields
  • Heat treating furnace linings
  • Flue stack and duct linings
  • Field steam generator linings

Information Provided by Unifrax I LLC

Vendors:
Available Properties
  • Density, Module
  • Density, Module
  • Maximum Service Temperature, Air, Recommended Operating Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Unifrax I LLC

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.